WSZL

Product description: PTFE bronze wiper seal WSZL

Beskriuwing

Tapassings en eigenskippen

For reciprocating system,especially in low temperature,high frequency and heavy dust conditions.

mainly applied to hydraulic and pneumatic devices,servo system,chemical and food

machinery.Excellent sliding performance,no stick-slip behavior,no viscosity,compensatesto the

distortion of pistons and plungers,excellent compatibility of hydraulic mediums,excellent effect of

scraping residue oil films of the rod surface from inside.

Standertmaterialen

Glidring: brûnsfol PTFE, koalstofvezelfol PTFE, grafytfol PTFE

O-ring: NBR/FKM. oar materiaal is beskikber.

3. Wurkbetingsten

Diameter Range: from 5mm to 1000mm

Drukberik: 0-60 MPa

Tempberik: -30℃ oant 200℃

Snelheid: <=5m/s

Medium: hydraulyske oalje, wetter, lucht, amper ûntflambere fluids.

other general seal profile name: WSZ2,DSZ2,DSZL

Freegje in offerte oan