Petearje mei ús, mooglik makke troch LiveChat

SPGO

Construction machinery seal
SPGO
Product description: Construction machinery seal SPGO

Beskriuwing

Applications and properties

SPGO,also called HBTS, is a standard double acting seal.For reciprocated hydraulic system,allow large extrusion gap,has wide application,high static and dynamic sealing effect,be able to work in dusty condition,low friction,available in various of materials.

Standard materials

Slide Ring:bronze filled PTFE,carbon fiber filled PTFE,graphite filled PTFE,Glass fiber filled PTFE

O-Ring:NBR/FKM. other material is available.

Working conditions

Diameter Range: from 3mm to 1000mm

Pressure Range:0-60 MPa

Temp Range: -45℃ to 200℃

Speed: <=15m/s

Medium:Hydraulic Oil,water,air barely flammable fluids.

Size:Standard and non-standard,please request.

Freegje in offerte oan