Beskriuwing

1. Applications and properties
Standard double acting seal.
For reciprocated hydraulic system,allow large extrusion gap,has wide application,high static and
dynamic sealing effect,be able to work in dusty condition,low friction,available in various of
materials,strong adaptability to work conditions.
2.Standard materials
Slide Ring:bronze filled PTFE,carbon fiber filled PTFE,graphite filled PTFE
O-Ring:NBR/FKM. other material is available.
3.Working conditions
Diameter
Bore diameter from 8 mm to 1600 mm
Other name: K08-D