E4 pneumatic piston seal has a special designed lip,it makes E4 keeps a good pre-lubricated effect,has been widely used.
Material&Temperature Range:
NBR:0℃ ~ 100 ℃; FKM:-20℃ ~ 220 ℃;
Hardness:70 shore A
Pressure:≤1.6 MPa
Speed:≤1m/s

| Part no.: | D | d | h | G | D1 |
| E4-14*8*4* | 14 | 8 | 4.0 | 4.5 | 13.0 |
| E4-16*10*4* | 16 | 10 | 4.0 | 4.5 | 15.0 |
| E4-22*18*4* | 22 | 18 | 4.0 | 4.5 | 21.0 |
| E4-24*16*5.5* | 24 | 16 | 5.5 | 6.0 | 23.0 |
| E4-25*17*5.5* | 25 | 17 | 5.5 | 6.0 | 24.0 |
| E4-32*24*5.5 | 32 | 24 | 5.5 | 6.0 | 31.0 |
| E4-40*30*7 | 40 | 30 | 7.0 | 7.5 | 38.5 |
| E4-42*30*6* | 42 | 30 | 6.0 | 6.5 | 40.5 |
| E4-45*33*9* | 45 | 33 | 9.0 | 9.5 | 31.5 |
| E4-50*40*7 | 50 | 40 | 7.0 | 7.5 | 48.5 |
| E4-63*53*7 | 63 | 53 | 7.0 | 7.5 | 61.5 |
| E4-80*68*8.5 | 80 | 68 | 8.5 | 9.5 | 78.0 |
| E4-99*88*9.8* | 99 | 88 | 9.8 | 10.8 | 97.0 |
| E4-100*88*8.25 | 100 | 88 | 8.5 | 9.5 | 98.0 |
| E4-120*105*10* | 120 | 105 | 10.0 | 11.0 | 117.5 |
| E4-125*110*10 | 125 | 110 | 10.0 | 11.0 | 122.5 |
| E4-150*135*10* | 150 | 135 | 10.0 | 11.0 | 147.5 |
| E4-160*145*10 | 160 | 145 | 10.0 | 11.0 | 157.5 |
| E4-200*180*14 | 200 | 180 | 14.0 | 15.0 | 195.0 |
| E4-250*230*14 | 250 | 230 | 14.0 | 15.0 | 245.0 |
| E4-320*295*17 | 320 | 295 | 17.0 | 18.0 | 312.5 |