Having been used very widerly in hydraulic cylinders, USH can be used for piston and rod applications because of having the height of both sealing lips equal.
Standardized with the materials of NBR 85 shore A, USH is also manufactured with Viton (FKM)material.
Datos técnicos
Pressure: 15 MPa
Temperatura:
NBR -35 to +105 ℃
FKM -35 to +200 ℃
Velocidad: 0,5 m/s
Medio: Aceites hidráulicos (a base de aceite mineral)
Material
Material: NBR / FKM
Hardness: 70-85 Shore A
Color: Black / Brown
Ventajas
Alta resistencia a altas temperaturas
Alta resistencia a la abrasión
Low compression set.
Fácil instalación