ODI/OSI

Product description: PISTON SEAL,PISTON U CUP,ODI/OSI

Descripción

ODI/OSI is a lip seal with a secondary sealing lip which can be used for both piston seal and rod seal.

Technical Data:
Pressure: below 400 Bar,
Temperature: -35  to +110℃
Speed: 0.5m/s
Media: Hydraulic oils (mineral oil-based)
Material: High-grade PU
Hardness: 90-95 Shore A
Color:Light yellow

Advantages

Insensibility against shock loads and pressure peaks
High resistance against extrusion
Perfect sealing performance under low pressure enven O-pressure
Easy installation

Solicitar presupuesto