Product description: PTFE Wiper Seal KZT

Descripción

Applications and properties

This product with the anti-wear and piston ring used in combination to prevent the cylinder oil mixed

with foreign matters and cause damage to the seals and to ensure that the seals have a long service life.The piston rod seals,used in combine with oil pressure,prevent to store up of oil pressure.

Standard materials

bronze filled PTFE,carbon fiber filled PTFE,graphite filled PTFE

Working conditions

Diameter Range: from 50 mm to 200 mm

Temp Range: -200℃ to +200℃

Speed: <=1.5 m/s

Medium:General petroleum based hydraulic oil,water/glycol hydraulic oil,oil/water emulsional,hydraulic oil.