DHS

wiper seal
PU wiper seal
rubber wiper seal
Product description: wiper seal DHS

Description

DHS wiper is a sealing element which used in hydraulic applications to obstruct all kinds of negative foreign particles to go into the cylinders.

Technical Data
Temperature: -35℃ to +100℃
Speed:  <=1m/s
Media: Hydraulic oils (mineral oil-based)

Material
Material: PU
Hardness: 70-90 Shore A
Color: Blue / Green

Advantages
High abrasion resistance.
Widely applicable.
Easy installation.