Anillo de respaldo de PEEK con carbono

Carbon fiber filled PEEK
Good bearing properties
Good wear properties
Balck gasket

Descripción

This gasket was made from carbon fiber filled PEEK,enhanced PEEK makes it has very good bearing and wear properties,suitable for automible industries and mechanical engineerings,etc.

Material:PEEK+30% carbon/PEEK+30% glass/PEEK+10% carbon+10% graphite+10% PTFE

Datos técnicos:

Temperatura:

Short time:+300 degree celsius

Long time:+260 degree ceelsius

Feature: Lubricant,good bearing and wear properties.

Color: Black