الوصف
This gasket was made from carbon fiber filled PEEK,enhanced PEEK makes it has very good bearing and wear properties,suitable for automible industries and mechanical engineerings,etc.
Material:PEEK+30% carbon/PEEK+30% glass/PEEK+10% carbon+10% graphite+10% PTFE
البيانات الفنية:
درجة الحرارة:
Short time:+300 degree celsius
Long time:+260 degree ceelsius
Feature: Lubricant,good bearing and wear properties.
Color: Black