Beschreibung
1. Anwendungen und Eigenschaften
Suitable for high-speed, high-pressure. With low friction and high elasticity, good dynamic and static sealing performance, groove is simple, good sliding. Recommended for piston-type accumulators, indicating double-acting pistons such as cylinders and positioning cylinders.
2. Standardwerkstoffe
Slide Ring:filled PTFE
O-Ring:NBR/FKM.
X-Ring:NBR/FKM.
3.Size
Bore dia from 16 mm to 1000mm
Other general seal profile name:DAQ2,JAQ2