Nylon back-up ring for U seal MBN, BRN3

Technische Daten:
Material: Nylon
Temperatur: -30℃ bis 100℃
Pressure: 0-30MPa
Speed: 1m/s
Nylon backup ring MBN BRN3 size
| Artikel | Größe mm |
| MBN/BRN3 | 35*50*3 |
| MBN/BRN3 | 40*50*3 |
| MBN/BRN3 | 40*55*3 |
| MBN/BRN3 | 45*55*3 |
| MBN/BRN3 | 50*60*3 |
| MBN/BRN3 | 50*63*3 |
| MBN/BRN3 | 55*65*3 |
| MBN/BRN3 | 55*68*3 |
| MBN/BRN3 | 55*70*3 |
| MBN/BRN3 | 60*70*3 |
| MBN/BRN3 | 60*73*3 |
| MBN/BRN3 | 60*80*3 |
| MBN/BRN3 | 64*80*3 |
| MBN/BRN3 | 65*75*3 |
| MBN/BRN3 | 65*80*3 |
| MBN/BRN3 | 65*80*3 |
| MBN/BRN3 | 65*85*3 |
| MBN/BRN3 | 70*80*3 |
| MBN/BRN3 | 70*83*3 |
| MBN/BRN3 | 70*85*3 |
| MBN/BRN3 | 75*85*3 |
| MBN/BRN3 | 75*88*3 |
| MBN/BRN3 | 75*90*3 |
| MBN/BRN3 | 75*95*3 |
| MBN/BRN3 | 80*90*3 |
| MBN/BRN3 | 80*93*3 |
| MBN/BRN3 | 80*95*3 |
| MBN/BRN3 | 80*100*3 |
| MBN/BRN3 | 85*100*3 |
| MBN/BRN3 | 85*105*3 |
| MBN/BRN3 | 90*105*3 |
| MBN/BRN3 | 90*110*3 |
| MBN/BRN3 | 95*110*3 |
| MBN/BRN3 | 95*115*3 |
| MBN/BRN3 | 100*115*3 |
| MBN/BRN3 | 100*120*3 |
| MBN/BRN3 | 105*120*3 |
| MBN/BRN3 | 105*125*3 |
| MBN/BRN3 | 110*125*3 |
| MBN/BRN3 | 110*130*3 |
| MBN/BRN3 | 115*130*3 |
| MBN/BRN3 | 115*135*3 |
| MBN/BRN3 | 120*135*3 |
| MBN/BRN3 | 120*140*3 |
| MBN/BRN3 | 130*145*3 |
| MBN/BRN3 | 130*150*3 |
| MBN/BRN3 | 140*160*3 |