تحدث معنا, ، مدعوم بواسطة LiveChat

ما هي مادة 56Si7؟ تركيب مادة 56Si7

شارك هذا المقال

ما هي مادة 56Si7؟ تركيب مادة 56Si7

For any request of 56si7 products,please contact us. Email: [email protected]

56Si7 carbon steel plate/56Si7 carbon steel round rod/56Si7 carbon steel strip

Material number: 1.5026
Brand: 56Si7
Standard: EN 10132-4:2000
Characteristics and applications:
56Si7 material, German grade special steel.

● Chemical composition:

Carbon C: 0.52-0.6
Silicon Si: 1.6-2
Manganese Mn: 0.6-0.9
Nickel Ni: ≤ 0.4
Phosphorus P: ≤ 0.025
Sulfur S: ≤ 0.025
Chromium Cr: ≤ 0.4
Molybdenum Mo: ≤ 0.1“

[56Si7 Steel Material Name]: Carbon steel, high-temperature alloy, precision alloy, carbon steel, cold heading steel, mold steel, bearing steel, composite steel, free cutting steel, spring steel, automotive steel plate

 [56Si7 steel material specifications]: thickness 0.5-300mm, whole plate specifications: 1220 * 2440mm, 1250mm * 2500mm, special specifications can be customized!

[56Si7 Steel Executive Standards]: Domestic GB/T, American ASTM, Japanese JIS, German DIN

Physical properties of 56Si7 steel: tensile strength, elastic modulus, plasticity, impact toughness, cold brittleness, hardness, cold bending performance, weldability, heat treatment, cold working and aging, etc

Origin of 56Si7 steel material: domestic and imported.

Main Markets for 56Si7 Steel: Various Industries

[56Si7 steel application field]: Manufacturing mechanical equipment, various tools, simple mechanical connecting rods, gears, couplings, pins and other parts

Minimum order quantity of 56Si7 steel: unlimited order quantity

56Si7 steel processing service: providing slitting, plate cutting, etc

اقرأ المزيد

شرح أطقم مانعات تسرب الأسطوانات الهيدروليكية: المكونات وفترات الاستبدال وكيفية الطلب الصحيح

ما يحتويه طقم مانعات تسرب الأسطوانة الهيدروليكية، والأطقم أحادية المفعول مقابل مزدوجة المفعول، والعمر الواقعي للمانعات حسب فئة الخدمة، وكيفية طلب الطقم الصحيح من الشركة المصنعة.