الوصف
التطبيقات:
GT-S is soft guide tape, it is widely used in hydraulic cylinders,pneumatic cylinders as rod piston guide elements.
المادة:
Brown:PTFE Bronze
Green:PTFE Bronze
Black:PTFE Carbon Fiber
Embossing:
Thickness more than or equal to 2mm can be supplied with embossing.
Embossing strucure is the sliding surface which with small lubrication micro cavity,it can promote the formation of a lubricant film,improve the micro-lubricating,embedded micro foreign matter and help to protect the seal system.
it can be generally made into a double-side embossing and single embossing.
Other general name:GST,BST,RYT