描述
防塵密封件 GA
遺傳算法 防塵密封件 can prevent dust,sand and other foreign matters goes into the cylinder,protected the metal slide face,improved the seal service life.protected the metal slide face,improved the seal service life.
Typical Applications
■Automotive: Engine crankshafts, transmissions, differentials.
■Industrial Equipment: Pumps, motors, gearboxes, bearing housings.
■Agricultural Machinery: Tractor drivetrains, harvester hydraulic systems.
技術數據:
溫度:-20至+100℃
Speed:≤ 15 m/s
介質:液壓油(礦物油基)
材料:
NBR+金屬,黑色
PU+金屬,金絲雀黃
GA dimensions
| 不。 | 尺寸 | 訂單號 | 不。 | 尺寸 | 訂單號 | |
| 1 | 16*26*7/10 | GA1626710 | 35 | 70*80*7/10 | GA7080710 | |
| 2 | 16*26*5/7 | GA162657 | 36 | 75*85*7/10 | GA7585710 | |
| 3 | 20*28*4/7 | GA202847 | 37 | 80*88*5/7 | GA808857 | |
| 4 | 20*30*7/10 | GA2030710 | 38 | 80*90*5/7 | GA809057 | |
| 5 | 22*32*7/10 | GA2232710 | 39 | 80*90*7/10 | GA8090710 | |
| 6 | 25*32*5/7 | GA253257 | 40 | 80*95*7/10 | GA8095710 | |
| 7 | 25*33*5/7 | GA253357 | 41 | 85*95*7/10 | GA8595710 | |
| 8 | 25*35*7/10 | GA2535710 | 42 | 90*100*7/10 | GA90100710 | |
| 9 | 28*36*5/7 | GA283657 | 43 | 90*105*7/10 | GA90105710 | |
| 10 | 28*38*5/8 | GA283858 | 44 | 100*110*7/10 | GA100110710 | |
| 11 | 28*38*7/10 | GA2838710 | 45 | 100*115*7/10 | GA100115710 | |
| 12 | 30*40*5/7 | GA304057 | 46 | 105*115*7/10 | GA105115710 | |
| 13 | 30*40*7/10 | GA3040710 | 47 | 110*120*7/10 | GA110120710 | |
| 14 | 32*40*7/10 | GA3240710 | 48 | 110*130*9/12 | GA110130912 | |
| 15 | 32*42*7/10 | GA3242710 | 49 | 110*125*7/10 | GA110125710 | |
| 16 | 32*45*5/7 | GA324557 | 50 | 120*130*7/10 | GA120130710 | |
| 17 | 32*45*7/10 | GA3245710 | ||||
| 18 | 35*45*5/7 | GA354557 | ||||
| 19 | 35*45*7/10 | GA3545710 | ||||
| 20 | 35*48*5/8 | GA354858 | ||||
| 21 | 36*45*7/10 | GA3645710 | ||||
| 22 | 36*46*5/7 | GA364657 | ||||
| 23 | 40*50*5/7 | GA405057 | ||||
| 24 | 40*50*7/10 | GA4050710 | ||||
| 25 | 42*52*7/10 | GA4252710 | ||||
| 26 | 45*55*5/7 | GA455557 | ||||
| 27 | 45*55*7/10 | GA4555710 | ||||
| 28 | 50*60*5/7 | GA506057 | ||||
| 29 | 50*60*7/10 | GA5060710 | ||||
| 30 | 50*62*7/10 | GA5062710 | ||||
| 31 | 55*65*7/10 | GA5565710 | ||||
| 32 | 60*70*7/10 | GA6070710 | ||||
| 33 | 63*75*5/8 | GA637558 | ||||
| 34 | 65*75*7/10 | GA6575710 |
我們是專業的工程機械備件密封件供應商,質量好,價格有競爭力,