Описание
DKBI/DKB Seals: Heavy-Duty Hydraulic Wiper
DKBI/DKB seals are metal-reinforced wipers designed to protect hydraulic cylinders from dirt, dust, and debris. Built with durable polyurethane (PU 93 Shore A) and a sturdy metal frame, they ensure long-lasting performance.

Key Features:
Temperature range: -35°C to +100°C
Speed tolerance: Up to 1 m/s
Compatibility: Works with standard mineral-based hydraulic oils.
Materials:
Main body: Wear-resistant PU or NBR rubber.
Metal frame for structural strength.
Color options: Blue, green, light yellow, or black.
Why Choose DKBI/DKB?
Excellent wear resistance for harsh environments.
Easy to install thanks to simple, user-friendly design.
Versatile use across construction, mining, and industrial machinery.
Dimensions:
| ID*OD*t/H (mm) | PU | PU | NBR | ID*OD*t/H (mm) | PU | PU | NBR | ID*OD*t/H (mm) | PU | PU |
| 13*19*4*5 | DKB | 38*50*7*10 | DKB | 65*79*8*12 | DKBI | |||||
| 14*22*4*7 | DKB | 40*50*7*10 | 66*80*8*10 | |||||||
| 18*30*6*9 | DKB | 40*50*7*12 | DKB | 68*90*10*14 | ||||||
| 19*26*5*7 | DKB | 40*52*6*9 | DKB | DKB | 70*80*7*10 | |||||
| 19*27*4*7 | DKB | 40*52*7*10 | DKBI | DKB | DKB | 70*80*8*11 | DKB | |||
| 19*31*6*9 | DKB | 40*62*8*11 | DKB | DKB | 70*84*8*11 | DKBI | DKB | |||
| 19*32*6*9 | DKB | 45*55*7*10 | DKB | 70*84*8*12 | DKBI | |||||
| 20*28*4*6 | DKB | 45*57*6*9 | DKB | DKB | 70*90*10*14 | |||||
| 20*30*4*6 | DKB | 45*57*7*10 | DKBI | DKB | 75*85*6*10 | DKB | ||||
| 20*32*6*9 | DKBI | DKB | DKB | 45*68*8*11 | DKB | 75*87*8*11 | DKB | |||
| 22*31.1*6.5*8 | DKB | 50*60*7*10 | DKB | 75*89*8*11 | DKBI | DKB | ||||
| 22*32*6*9 | DKB | 50*62*6*9 | DKB | DKB | 75*89*8*12 | DKBI | ||||
| 22*34*6*9 | DKB | DKB | 50*62*7*10 | DKBI | DKB | DKB | 80*90*8*11 | DKB | ||
| 25*37*6*9 | DKBI | DKB | DKB | 50*64*7*10 | DKB | 80*92*7*10 | DKB | |||
| 28*40*6*9 | DKBI | DKB | 50*64*8*12 | DKB | 80*94*8*11 | DKBI | DKB | |||
| 30*42*6*9 | DKBI | DKB | DKB | 50*72*8*11 | DKB | 80*94*8*12 | DKBI | |||
| 30*47*7*10 | DKB | 55*69*7*10 | DKB | DKB | 80*95*6*7.5 | |||||
| 32*39*5*9 | DKB | 55*69*8*11 | DKBI | DKB | 85*99*8*11 | DKBI | DKB | |||
| 32*44*6*9 | DKB | DKB | 55*69*8*12 | DKBI | 85*99*8*12 | DKBI | ||||
| 32*44*7*10 | DKB | 60*70*7*10 | DKB | 90*104*8*11 | DKBI | DKB | ||||
| 32*52*7*10 | DKB | 60*74*7*10 | DKB | DKB | 90*104*8*12 | DKBI | ||||
| 32*52*8*11 | DKB | 60*74*8*11 | DKBI | DKB | 95*104*8*11 | |||||
| 34*46*7*10 | DKB | 60*74*8*12 | DKBI | 95*107*8*11 | DKB | |||||
| 35*47*6*9 | DKB | 60*82*8*11 | DKB | 95*109*8*11 | DKBI | DKB | ||||
| 35*47*7*10 | DKBI | DKB | DKB | 65*79*8*11 | DKBI | DKB | DKB | 95*109*8*12 | DKBI |
| ID*OD*t/H (mm) | PU | PU | NBR |
| 100*114*8*11 | DKBI | DKB | DKB |
| 100*114*8*12 | DKBI | ||
| 104*114*6*10 | DKB | ||
| 105*115*7*10 | DKB | ||
| 105*121*8*11 | DKB | DKB | |
| 105*121*9*12 | DKBI | DKB | |
| 105*121*9*12.5 | DKBI | ||
| 110*126*9*12 | DKBI | DKB | DKB |
| 110*126*9*12.5 | DKBI | ||
| 115*127*8*11 | DKB | ||
| 115*131*9*12 | DKBI | DKB | DKB |
| 115*131*9*12.5 | DKBI | ||
| 120*136*9*12 | DKBI | DKB | DKB |
| 120*136*9*12.5 | DKBI | ||
| 125*141*9*12 | DKBI | DKB | |
| 125*141*9*12.5 | DKBI | ||
| 125*141*10*14 | DKB | ||
| 129*139*6*10 | DKB | ||
| 130*146*9*12 | DKBI | DKB | |
| 130*146*9*12.5 | DKBI | ||
| 130*146*10*14 | DKB | DKB | |
| 140*155*9*11 | DKB | ||
| 140*160*10*14 | DKBI | DKB | DKB |
| 145*165*10*14 | DKB | DKB | |
| 150*170*10*14 | DKBI | DKB | DKB |
| 160*180*10*14 | DKBI | DKB | DKB |
| 170*190*10*14 | DKBI | DKB | DKB |
| 175*195*10*14 | DKB | DKB | |
| 180*200*10*14 | DKBI | DKB | DKB |
| 180*205*12*17 | DKB | ||
| 210*235*12*17 | DKB | ||
| 265*285*12*17 | DKB | ||
For other sizes,please request us.