What is 56Si7 material? 56Si7 material composition

Share This Post

What is 56Si7 material? 56Si7 material composition

For any request of 56si7 products,please contact us. Email: [email protected]

56Si7 carbon steel plate/56Si7 carbon steel round rod/56Si7 carbon steel strip

Material number: 1.5026
Brand: 56Si7
Standard: EN 10132-4:2000
Characteristics and applications:
56Si7 material, German grade special steel.

● Chemical composition:

Carbon C: 0.52-0.6
Silicon Si: 1.6-2
Manganese Mn: 0.6-0.9
Nickel Ni: ≤ 0.4
Phosphorus P: ≤ 0.025
Sulfur S: ≤ 0.025
Chromium Cr: ≤ 0.4
Molybdenum Mo: ≤ 0.1“

[56Si7 Steel Material Name]: Carbon steel, high-temperature alloy, precision alloy, carbon steel, cold heading steel, mold steel, bearing steel, composite steel, free cutting steel, spring steel, automotive steel plate

 [56Si7 steel material specifications]: thickness 0.5-300mm, whole plate specifications: 1220 * 2440mm, 1250mm * 2500mm, special specifications can be customized!

[56Si7 Steel Executive Standards]: Domestic GB/T, American ASTM, Japanese JIS, German DIN

Physical properties of 56Si7 steel: tensile strength, elastic modulus, plasticity, impact toughness, cold brittleness, hardness, cold bending performance, weldability, heat treatment, cold working and aging, etc

Origin of 56Si7 steel material: domestic and imported.

Main Markets for 56Si7 Steel: Various Industries

[56Si7 steel application field]: Manufacturing mechanical equipment, various tools, simple mechanical connecting rods, gears, couplings, pins and other parts