Product description: PTFE V packs,ptfe vee pack,ptfe v packing,ptfe v packing

Description

This V packs,including the support ring, the seal ring and the pressure ring are all made of pure polytetrafluoroethylene(PTFE) material, worked as piston seals in reciprocating applications.

The vee packing has low friction coefficient, high temperature resistance and chemical resistance. It is widely used in pumps, metallurgy, mining equipment, general machinery and so on.

Pressure <60MPa

Temperature: -60 ° C / +260 ° C

Size: can be customized according to specific working conditions