Chatta con noi, offerto da LiveChat

Descrizione

UNR/UHR are used very widely in hydraulic cylinders.  Having shorter inner sealing lip,UNR/UHR nut rings are designed especially for rod applications.

Technical Data
Pressure:  400 Bar
Temperature: -35  to +100
Speed:  0.5m/s
Media: Hydraulic oils (mineral oil-based)

Material
Material: PU
Hardness: 93 Shore A
Color: Blue, Dark green

Advantages
High resistance to high temperature
High abrasion resistance
Low compression set

Easy installation

Richiedi un preventivo

Contattaci oggi stesso e ricevi una revisione aziendale e una consulenza gratuite.