Custom LNG CNG SEAL
Stainless spring energized UHMWPE(UPE) jacket seal, yellow or white color, 32.8*40*5mm
PCTFE gasket, translucent color, 5*25*2mm
Properties: Low temperature resistance,Wear resistance,Corrosion resistance
Pressure: below 45 MPa
Speed:<15 m/s
Stock:Yes