- PTFE Encapsulated Seals
- Rubber O-Ring,X-Ring
- Spring Energized Seals/Vari Seal
- Hydraulic Rod&Piston Seals
- Hydraulic Piston Seals
- Hydraulic Rod Seals
- Hydraulic Wiper Seals
- Rotary Seals
- Guiding Elements
- Gasket washers Back-up Ring
- Pneumatic Seals& Pneumatic Seal Kits
- Seal Kits
- High-Temperature&Low Temperature Seals
- Rubber Seals
- Oil Seals
- Engineering Plastics Products
- Customized Products
- Add: Nanbian Ave,Sanshui District,Guangdong,China
- Tel: +86 757 87333601
- Fax: +86 757 87333601
- Email: [email protected]



PTFE O-Ring
- White color
- Food grade available
- virgin pure PTFE
- CNC O RING
- Product description: PTFE O-RING
Product introduction
PTFE O Ring is a popular material which used in chemical resistant and non-compressible applications.Pure PTFE O Ring is white color.
Polytetrafluoroethylene (PTFE) is used wherever the chemical and thermal resistance of the elastomer O-Rings is no longer sufficient. These are primarily applications in the chemical, food, pharmaceuticals and medical industries. PTFE is used only as static seals, e.g. on flanges, covers, etc.
PTFE has the highest resistance to chemicals of all the plastics and can be used for almost any application. It has limited resistance to molten alkaline metals, to elementary fluorine and to certain halogen compounds. PTFE undergoes no changes on exposure to aging, light and ozone. The water absorption rate is less than 0.01%.
Applications:
It is resistant to most chemicals including acids, bases, oils, steam and other chemicals. It is also very tough and abrasive resistant. However the material is not easily compressed, and therefore may not seal as easily as some of the other polymers. Its outstanding tear resistance and abrasive resistance result in its slippery surface properties that make it advantageous for use in seals in moving systems such as mass spectrometer probes and valves.
Technical Data
Operating Temperature: -200 ℃ to 260℃
Size:Any size available.
Manufacturing process: CNC and Mould pressing.