- PTFE Encapsulated Seals
- Rubber O-Ring,X-Ring
- Spring Energized Seals/Vari Seal
- Hydraulic Rod&Piston Seals
- Hydraulic Piston Seals
- Hydraulic Rod Seals
- Hydraulic Wiper Seals
- Rotary Seals
- Guiding Elements
- Gasket washers Back-up Ring
- Pneumatic Seals& Pneumatic Seal Kits
- Seal Kits
- High-Temperature&Low Temperature Seals
- Rubber Seals
- Oil Seals
- Engineering Plastics Products
- Customized Products
- Add: 3906,Dxing road,Sanshui,Foshan City,528100,Guangdong,China
- Tel: +86 757 87333601
- Fax: +86 757 87333601
- Email: [email protected]



KDAS
- KDAS
- DDAS
- DAS
- Product description: Compact Seal KDAS
Product introduction
Applications and properties
DDAS/KDAS compact seal is a double acting seal and guide element,it is consist of 1 piece elastomer ring,2 pieces back up rings and 2 pieces guide rings. Elastomer has an good sealing effect in both dynamic and static conditions,back up ring prevent the elastomer be extruded into the sealing gap.
the role of the guide ring is to help the piston in the cylinder guide and absorb the radial force.
it mainly used in hydraulic cylinders as a piston seal.
Application:
Bulldozers, excavators, loaders, cranes, hydraulic gate and agricultural machinery.
Standard materials
Guide ring:POM
Back-up ring:PU
Elastomer:NBR
Working conditions
Diameter Range: from 20mm to 250mm
Pressure Range:0-35 MPa
Temp Range: -30℃ to 120℃
Speed: <=0.5m/s
Medium:Hydraulic Oil,water,air barely flammable fluids.
Size:Standard