- PTFE Encapsulated Seals
- Rubber O-Ring,X-Ring
- Spring Energized Seals/Vari Seal
- Hydraulic Rod&Piston Seals
- Hydraulic Piston Seals
- Hydraulic Rod Seals
- Hydraulic Wiper Seals
- Rotary Seals
- Guiding Elements
- Gasket washers Back-up Ring
- Pneumatic Seals& Pneumatic Seal Kits
- Seal Kits
- High-Temperature&Low Temperature Seals
- Rubber Seals
- Oil Seals
- Engineering Plastics Products
- Customized Products
- Add: Nanbian Ave,Sanshui District,Guangdong,China
- Tel: +86 757 87333601
- Fax: +86 757 87333601
- Email: [email protected]
Rubber SealsYour position: Home > Rubber Seals



V-RING TYPE A
- V-RING A
- VA RUBBER SEAL
- NBR/FKM
- Waterproof and oilproof
- Product description:
Product introduction
V-ring type A is a common non-pressure elastic rubber sealing ring for rotating shaft. The sealing lip has good mobility and adaptability. It can compensate for large tolerances and angular deviations and prevent the intrusion of external water and dust.The VA type seal can be used for sealing and repairing and repairing the main product. It is common in the anti-cold seal of washing equipment and rolling bars.
V ring A dimensions:
Size | Φd1 | Φd | c | A | B | Φd2 | Φd3 | Assembly width B1 |
VA-3 | 2.7-3.5 | 2.5 | 1.5 | 2.1 | 3 | d1+1 | d1+6 | 2.5±0.3 |
VA-4 | 3.5-4.5 | 3.2 | 2 | 2.4 | 3.7 | d1+1 | d1+6 | 3±0.4 |
VA-5 | 4.5-5.5 | 4 | 2 | 2.4 | 3.7 | d1+1 | d1+6 | 3±0.4 |
VA-6 | 5.5-6.5 | 5 | 2 | 2.4 | 3.7 | d1+1 | d1+6 | 3±0.4 |
VA-7 | 6.5-8 | 6 | 2 | 2.4 | 3.7 | d1+1 | d1+6 | 3±0.4 |
VA-8 | 8-9.5 | 7 | 2 | 2.4 | 3.7 | d1+1 | d1+6 | 3±0.4 |
VA-10 | 9.5-11.5 | 9 | 3 | 3.4 | 5.5 | d1+1 | d1+9 | 4±0.6 |
VA-12 | 11.5-13.5 | 10.5 | 3 | 3.4 | 5.5 | d1+1 | d1+9 | 4±0.6 |
VA-13 | 12.5-13.5 | 11.7 | 3 | 3.4 | 5.5 | d1+1 | d1+9 | 4±0.6 |
VA-14 | 13.5-15.5 | 12.5 | 3 | 3.4 | 5.5 | d1+1 | d1+9 | 4±0.6 |
VA-16 | 15.5-17.5 | 14 | 3 | 3.4 | 5.5 | d1+1 | d1+9 | 4±0.6 |
VA-18 | 17.5-19 | 16 | 3 | 3.4 | 5.5 | d1+1 | d1+9 | 4±0.6 |
VA-20 | 19-21 | 18 | 4 | 4.7 | 7.5 | d1+2 | d1+12 | 6±0.8 |
VA-22 | 21-24 | 20 | 4 | 4.7 | 7.5 | d1+2 | d1+12 | 6±0.8 |
VA-25 | 24-27 | 22 | 4 | 4.7 | 7.5 | d1+2 | d1+12 | 6±0.8 |
VA-28 | 27-29 | 25 | 4 | 4.7 | 7.5 | d1+2 | d1+12 | 6±0.8 |
VA-30 | 29-31 | 27 | 4 | 4.7 | 7.5 | d1+2 | d1+12 | 6±0.8 |
VA-32 | 31-33 | 29 | 4 | 4.7 | 7.5 | d1+2 | d1+12 | 6±0.8 |
VA-35 | 33-36 | 31 | 4 | 4.7 | 7.5 | d1+2 | d1+12 | 6±0.8 |
VA-38 | 36-38 | 34 | 4 | 4.7 | 7.5 | d1+2 | d1+12 | 6±0.8 |
VA-40 | 38-43 | 36 | 5 | 5.5 | 9 | d1+2 | d1+15 | 7±1 |
VA-45 | 43-48 | 40 | 5 | 5.5 | 9 | d1+2 | d1+15 | 7±1 |
VA-50 | 48-53 | 45 | 5 | 5.5 | 9 | d1+2 | d1+15 | 7±1 |
VA-55 | 53-58 | 49 | 5 | 5.5 | 9 | d1+2 | d1+15 | 7±1 |
Size | Φd1 | Φd | c | A | B | Φd2 | Φd3 | Assembly width B1 |
VA-60 | 58-63 | 54 | 5 | 5.5 | 9 | d1+2 | d1+15 | 7±1 |
VA-65 | 63-68 | 58 | 5 | 5.5 | 9 | d1+2 | d1+15 | 7±1 |
VA-70 | 68-73 | 63 | 6 | 6.8 | 11 | d1+3 | d1+18 | 9±1.2 |
VA-75 | 73-78 | 67 | 6 | 6.8 | 11 | d1+3 | d1+18 | 9±1.2 |
VA-80 | 78-83 | 72 | 6 | 6.8 | 11 | d1+3 | d1+18 | 9±1.2 |
VA-85 | 83-88 | 76 | 6 | 6.8 | 11 | d1+3 | d1+18 | 9±1.2 |
VA-90 | 88-93 | 81 | 6 | 6.8 | 11 | d1+3 | d1+18 | 9±1.2 |
VA-95 | 93-98 | 85 | 6 | 6.8 | 11 | d1+3 | d1+18 | 9±1.2 |
VA-100 | 98-105 | 90 | 6 | 6.8 | 11 | d1+3 | d1+18 | 9±1.1 |
VA-110 | 105-115 | 99 | 7 | 7.9 | 12.8 | d1+4 | d1+21 | 10.5±1.5 |
VA-120 | 115-125 | 108 | 7 | 7.9 | 12.8 | d1+4 | d1+21 | 10.5±1.5 |
VA-130 | 125-135 | 117 | 7 | 7.9 | 12.8 | d1+4 | d1+21 | 10.5±1.5 |
VA-140 | 135-145 | 126 | 7 | 7.9 | 12.8 | d1+4 | d1+21 | 10.5±1.5 |
VA-150 | 145-155 | 135 | 7 | 7.9 | 12.8 | d1+4 | d1+21 | 10.5±1.5 |
VA-160 | 155-165 | 144 | 8 | 9 | 14.5 | d1+4 | d1+24 | 12±1.8 |
VA-170 | 165-175 | 153 | 8 | 9 | 14.5 | d1+4 | d1+24 | 12±1.8 |
VA-180 | 175-185 | 162 | 8 | 9 | 14.5 | d1+4 | d1+24 | 12±1.8 |
VA-190 | 185-195 | 171 | 8 | 9 | 14.5 | d1+4 | d1+24 | 12±1.8 |
VA-199 | 195-210 | 180 | 8 | 9 | 14.5 | d1+4 | d1+24 | 12±1.8 |
VA-200 | 190-210 | 180 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-220 | 210-235 | 198 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-250 | 235-265 | 225 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-275 | 265-290 | 247 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-300 | 290-310 | 270 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-325 | 310-335 | 292 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-350 | 335-365 | 315 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-375 | 365-390 | 337 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-400 | 390-430 | 360 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-450 | 430-480 | 405 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-500 | 480-530 | 450 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-550 | 530-580 | 495 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-600 | 580-630 | 540 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-650 | 630-665 | 600 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-700 | 665-705 | 630 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-725 | 705-745 | 670 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-750 | 745-785 | 705 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-800 | 785-830 | 745 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-850 | 830-870 | 785 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-900 | 875-920 | 825 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-950 | 920-965 | 865 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-1000 | 965-1015 | 910 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
VA-1050 | 1015-1065 | 955 | 15 | 14.3 | 25 | d1+10 | d1+45 | 20±4 |
For further information,please request.