Having shorter outer sealing lip,UNP/UHP are desinged especially for piston applications.It is a lip-seal which fits tightly in the groove.

Technical Data:
Pressure:  400 bar
Temperature: -35 ℃ to +110℃
Speed: 0.5m/s
Media: Hydraulic oils (mineral oil-based)
Material: PU
Hardness: 90-95 Shore A
Color: Nature/Blue/Green


Advantages
Insensibility against shock loads and pressure peaks
High resistance against extrusion
Perfect sealing performance under low pressure enven O-pressure
Easy installation