Welcome: BOSS Sealing Solutions
Language: Chinese ∷  English

Hydraulic Piston Seals

  • OUY
OUY

OUY

  • oil seal
  • hydraulic compact piston seal
  • Material:NBR+PA
  • Application:Constrution machinery
  • Product description:
  • INQUIRY

OUY OIL SEAL

OUY is mainly used for piston seals of tensioning cylinders of construction machinery such as forklifts, excavators, etc.Has the characteristics of wear resistance, high pressure resistance, aging resistance, corrosion resistance.

Technical Data:    
Pressure:  ≤30 MPa   
Temperature: -20℃ to +100℃    
Speed: 0.5m/s  
Material: NBR+PA

Sizes:

OD*ID*H (mm)
40*25*12
50*35*12
60*45*12
60*35*15.5
65*50*12
70*54*12
70*55*12
70*40*12
70*45*15.5
70*90*12
75*65*8
75*60*12
80*64*12
80*50*12
80*47*16
90*70*15
90*80*8
85*70*12
90*65*18
100*75*18
105*90*12
110*90*12
105*85*12
100*80*12
130*110*12
150*130*12
120*100*12