  • Product description: UHMWPE seal,UPE lip seal, uhmwpe spring seal,low temperature seal
  • INQUIRY
UHMWPE has excellent impact resistance, wear resistance, chemical corrosion resistance, low friction coefficient, self-lubricating property, excellent mechanical properties in ultra-low temperature environment, and better wear resistance than PTFE. Sex and creep resistance. The disadvantages are insufficient tensile strength, poor high temperature resistance, low hardness and low thermal conductivity.

Material: UHMWPE/UPE+ Stainless Steel Spring
Working temperature: -180 ° C ~ +70 ° C

Working condition:
It is recommended for use in ultra-low temperature environments where it is recommended to have high sliding performance requirements or poor lubricity, high wear resistance requirements, or dry friction in medium water.