Applications and properties

For both high and low speed reciprocated hydraulic system.

Possessing excellent performance in argoing fluid and high temperature conditions.


Standard materials

Slide Ring:bronze filled PTFE,carbon fiber filled PTFE,graphite filled PTFE

O-Ring:NBR/FKM. other material is available.


Working conditions

Diameter Range: from 3mm to 1000mm

Pressure Range:0-60 MPa

Temp Range: -45℃ to 200℃

Speed: <=15m/s

Medium:Hydraulic Oil,water,air barely flammable fluids.



Other general seal profile name:GSI,DSI