  • Product description: HYDRAULIC ROD SEAL R2
  • INQUIRY

R2 is a standard seal profile of hallite H605, it operates well in every hydraulic applications.

Technical Data
Pressure: below 400 Bar,
Temperature: -35  to +110℃
Speed: 0.5m/s
Media: Hydraulic oils (mineral oil-based)
Material: High-grade PU
Hardness: 90-95 Shore A
Color:Blue/Green

Advantages:

Insensibility against shock loads and pressure peaks
High resistance against extrusion
Perfect sealing performance under low pressure enven O-pressure
Easy installation