  • Product description: PTFE Wiper Seal WPT2
  • INQUIRY

1. Applications and properties

Used in agricultural machinery,injection molding machines,forklifts,cranes.

Including one PTFE slide ring and two o-ring energizer,scraper seal DPT2 improves the sealing

effect,lowcoefficient offriction,no stick-slip behavior.Excellent performance in locating and

positioning.

Especially suitable for large diameter hydraulic cylinders.


2.Standard materials

Slide Ring:bronze filled PTFE,carbon fiber filled PTFE,graphite filled PTFE

O-Ring: NBR/FKM. other material is available.


3.Working conditions

Diameter Range: from 100 mm to 1000 mm

Pressure Range:0-60 MPa

Temp Range: -30℃ to 200℃

Speed: <=5m/s

Medium:Hydraulic Oil,water,air barely flammable fluids.