  • Product description: PISTON SEAL KR
  • INQUIRY

KR is a double-acting piston seal,the most pressure is 300bar.KR compact is consist of a PU slide ring and a NBR elatomer element.

Technical Data
Pressure: 300 bar
Temperature: -35  to +110℃
Speed:  0.5m/s
Media: Hydraulic oils (mineral oil-based)

Material
Material: PU + NBR


Advantages:

Insensibility against shock loads and pressure peaks
High resistance against extrusion
Perfect sealing performance under low pressure enven O-pressure
Easy installation