- PTFE Encapsulated Seals
- Rubber O-Ring,X-Ring
- Spring Energized Seals/Vari Seal
- Hydraulic Rod&Piston Seals
- Hydraulic Piston Seals
- Hydraulic Rod Seals
- Hydraulic Wiper Seals
- Rotary Seals
- Guiding Elements
- Gasket washers Back-up Ring
- Pneumatic Seals& Pneumatic Seal Kits
- Seal Kits
- High-Temperature&Low Temperature Seals
- Rubber Seals
- Oil Seals
- Engineering Plastics Products
- Customized Products
- Add: 3906,Dxing road,Sanshui,Foshan City,528100,Guangdong,China
- Tel: +86 757 87333601
- Fax: +86 757 87333601
- Email: [email protected]



Encapsulated Camlock Gaskets
- FEP/PFA encapsulated
- Silicone or FKM core
- Encapsulated Square gasket
- Coated rectangle gasket
- Product description: PTFE FEP Encapsulated Silicone Gasket,FEP Encapsulated VMQ Gasket,PFA Encapsulated Silicone Gasket,Teflon PFA Encapsulated VMQ Gasket
Product introduction
The cross sectional shape of encapsulated gaskets is rectangle or square, material is same as encapsulated o-rings,consist of transparent seamless FEP or PFA shell and VMQ or FKM elastomer core.
Advantage and standard material choosing ,please refer encapsulated o-ring.
Hollow core silicone or FKM rubber available.
Versions:
◎FEP encapsulated VMQ gasket;
◎FEP encapsulated FKM gasket;
◎PFA encapsulated VMQ gasket;
◎PFA encapsulated FKM gasket;
Encapsulated cam lock gasket standard sizes
1" , 1-1/4" , 1-1/2" , 2", 2-1/2" , 3" , 4" , 5" , 6" , 8"
Other lager sizes are available,such as 4780mm*14mm*14mm.
For further details,please request us.