Technical Data
Temperature: -35℃ to +100℃
Speed: <=1m/s
Media: Hydraulic oils (mineral oil-based)
Material
Material: PU
Hardness: 70-90 Shore A
Color: Blue / Green
Advantages
High abrasion resistance.
Widely applicable.
Easy installation.