Beschreibung

Applications and properties
For both high and low speed reciprocated hydraulic system.
Possessing excellent performance in argoing fluid and high temperature conditions.
Standard materials
Gleitring: bronzegefülltes PTFE, kohlenstofffasergefülltes PTFE, graphitgefülltes PTFE
O-Ring: NBR/FKM. Andere Werkstoffe sind erhältlich.
Working conditions
Diameter Range: from 3mm to 1000mm
Pressure Range:0-60 MPa
Temp Range: -45℃ to 200℃
Speed: <=15m/s
Medium: Hydrauliköl, Wasser, Luft, schwer entflammbare Fluide.
Other general seal profile name:GSI,DSI