Beschreibung

1. Anwendungen und Eigenschaften
Used in agricultural machinery,injection molding machines,forklifts,cranes.
Including one PTFE slide ring and two o-ring energizer,scraper seal DPT2 improves the sealing
effect,lowcoefficient offriction,no stick-slip behavior.Excellent performance in locating and
positioning.
Especially suitable for large diameter hydraulic cylinders.
2. Standardwerkstoffe
Gleitring: bronzegefülltes PTFE, kohlenstofffasergefülltes PTFE, graphitgefülltes PTFE
O-Ring: NBR/FKM. other material is available.
3. Einsatzbedingungen
Diameter Range: from 100 mm to 1000 mm
Pressure Range:0-60 MPa
Temp Range: -30℃ to 200℃
Speed: <=5m/s
Medium: Hydrauliköl, Wasser, Luft, schwer entflammbare Fluide.
Other seal profile name: DPT2,PT2,DPR