B7/UP is a lip seal which fits tightly in the groove.These seals may be used for all applications where the physical properties of normal or fabric elasstomers are insufficient.
Technical Data:
Pressure: below 400 Bar,
Temperature: -35 to +110℃
Speed: 0.5m/s
Media: Hydraulic oils (mineral oil-based)
Material: High-grade PU
Hardness: 90-95 Shore A
Color:Green,Blue
Advantages
Insensibility against shock loads and pressure peaks
High resistance against extrusion
Perfect sealing performance under low pressure enven O-pressure
Easy installation